05-28-2005 05:44 PM #3
brian, first of all what type of primer did you use under the sikkins?
If its was a 2K product , you can shoot a few coats over the sanded lifting area like HRP said , I would let it sit 24 hours , then water sand the whole panel with 600-800 grit. That should hold down the broken clear edge to allow you to get color layed down.
OR see if sikkins has a non sanding catylized sealer that will work .
What temp reducer are you using in the base?
May try a faster drying temp so it doesnt attack that edge so bad.
I thought you had a Sikkins master to see and show you what needed to be done to correct your problem?